Li Nb O 3 -doped (Na,K)NbO3 lead-free piezoelectric ceramics were prepared by normal sintering, and the electrical properties were investigated with a special emphasis on the influence of sintering temperature. The ceramics synthesized at 1020–1080°C showed a phase transition from orthorhombic to tetragonal symmetry, which is similar to the morphtropic phase boundary (MPB). Because of such MPB-like behavior, a high piezoelectric coefficient d33 (314pC∕N) was obtained in the nominal composition 0.058LiNbO3–0.942[(Na0.535K0.480)NbO3] ceramic sintered at 1060°C; however, this high d33 value was reported previously only in the Li-modified (Na,K)NbO3-based ceramics with codopants of Ta and Sb to B site.