Abstract
High performance thin film transistor (TFT) with atomic layer deposition (ALD) nitrogen doped ZnO (ZnO:N) as an active layer is demonstrated. The electrical properties of ZnO thin films were effectively controlled by in situ nitrogen doping using NH4OH as a source for reactants. Especially, the electron concentration in ZnO was lowered to below 1015cm−3. Good device characteristics were obtained from the inverted staggered type TFTs with ZnO:N channel and ALD Al2O3 gate insulator; μsat=6.7cm2∕Vs, Ioff=2.03×10−12A, Ion∕off=9.46×107, and subthreshold swing=0.67V∕decade. The entire TFT fabrication processes were carried out at below 150°C, which is a favorable process for plastic based flexible display.