Abstract

Macroporous, low-density polyetheretherketone, polyetherketoneketone, and polyetherimide foams are produced using a high-temperature, thermally induced phase separation method. A high-boiling-point solvent, which is suitable to dissolve at least 20 wt% of these high-performance polymers at temperatures above 250 °C, is identified. The foam morphology is controlled by the cooling procedure. The resulting polymer foams have porosities close to 80% with surface areas up to 140 m2 g-1 and elastic moduli up to 97 MPa.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.