Abstract

In this paper an attempt has been made to investigate the performance of an electrode made through powder metallurgy (PM) of copper tungsten during electrical discharge machining (EDM). Experimental results are presented on electrical discharge machining of AISI D2 hardened steel in kerosene with a copper tungsten (Cu35% - W65%) tool electrode made through PM method with a constant duty factor of 80%. In term of high performance EDM process, higher peak current (>20A) and pulse duration (>400µs) with a high machining efficiency were used. Experimental results have shown that machining at a peak current of 40A and pulse duration of 400µs yields the highest material removal rate (MRR) whereas machining at a peak current of 20A and pulse duration of 400µs yields the lowest tool wear rate (TWR). The lowest surface roughness appears at the lowest material removal rate which is at a peak current of 20A and pulse duration of 600µs. The optimum machining performance can be performed by the combination of pulse duration and peak current at 600µs and 40A respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.