Abstract

Highly stable and high performance solution-processed amorphous oxide semiconductor thin film transistors (TFTs) were produced using a Li and Zr co-doped ZnO-based aqueous solution. Li and Zr co-doping at the appropriate amounts enhanced the oxide film quality in terms of enhanced oxygen bonding and reduced defect sites. The 0.5 mol% Li and 1.0 mol% Zr co-doped ZnO TFTs annealed at 320 °C exhibited noticeably lower threshold voltage shifts of 3.54 V under positive bias stress and −2.07 V under negative bias temperature stress than the non-doped ZnO TFTs. The transistors revealed a good device mobility performance of 5.39 cm2 V−1 s−1 and an on/off current ratio of 108 when annealed at 320 °C, compared to a mobility performance of 2.86 cm2 V−1 s−1 and an on/off current ratio of ∼107 when annealed at 270 °C. Our results suggest that Li and Zr co-doping can be a useful technique to produce more reliable and low temperature solution-processed oxide semiconductor TFTs.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.