Abstract

Electroplating was the process of coating metal surfaces using the electrochemical method. We used alkaline zinc (Zn2+) plating that was anti-corrosion coating, cheapest, evenly adhesion, as well as better-looking crushing. This study aims to test and measure the thickness of the layer on spark plugs with variations in different electrical currents 300, 400, and 500A and increased hours during the coating process, investigate the corrosion resistance of white rust on the surface and analyze the changes in alkaline zinc concentration and temperature that affect the thickness of the layer, respectively. The results, such as 1st sample 13 pcs, 300A, and thickness of 7.26-micron with white rust 9 pcs. 2nd sample 13 pcs, 400A, and thickness of 9.15-micron white rust 5 pcs. 3rd sample 13 pcs, 500A, and thickness of 12.75-micron white rust 3 pcs. The high electric current (500A) and 45 hours of the experiment would influence the lowest white rust corrosion level. The high alkaline zinc solution with an optimum 36°C solution temperature and 500A electric current would undoubtedly deposit the white rust until 3 pcs.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.