The Ni-rich LiNi0.8 Co0.10 Mn0.1 O2 (NCM811) cathode coated by combining with multi-walled carbon nanotubes (MWCNTs) and polyimide (PI) produces a PI3-NCM811 cathode, which markedly improves cycling stability and suppresses secondary crystal cracking. The initial discharge capacity of the PI3-NCM811 cathode is 199.6 mAh g-1 between 2.8 and 4.3V at 0.1 C @ 25 °C, which is slightly lower than that of NCM811 (201.1 mAh g-1 ). The PI3-NCM811 and NCM811 cathodes keep 90.6% and 64.8% of their initial discharge capacity at 1 C between 2.8 and 4.3 Vafter 500 cycles, respectively. Furthermore, the difference (21.1%) in capacity retention rate between PI3-NCM811 and NCM811 under the condition of 2.8-4.5 Vbecame smaller compared with the difference (25.8%) under the condition of 2.8-4.3 V.This better cyclic stability is mainly attributed to the toughness and elasticity of PI, which inhibits the secondary cracking, maintains the structural integrity of the cathode particles, and protects the particles from electrolyte damage during long-term cycling.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.