It is an urgent need to develop efficient solid state cooling technologies and materials with high cycle life. Poly-p-phenylene benzodioxole (PBO) is a high performance fiber with excellent mechanical properties. In this work, for the first time, elasto- and twistocaloric cooling of PBO fibers by stretching and twisting of the PBO fiber bundles is reported. The cooling temperature reaches -0.4 and -1.3 K, for fiber stretching and twisting, respectively. A self-coiled PBO fiber achieves maximum cooling of -3.7K upon stretching by 35% strain, with an exceptionally high cycle life of 200000 times. During the twisting of the PBO fibers, reversible changes in the intensity of the diffraction peaks in X-ray diffraction patterns are observed. A strain-sensitive color change application is realized by coating a self-coiled PBO fiber with liquid crystallite dyes. This work provides new perspectives for PBO fibers as a high cycle-life solid-state refrigeration material.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.