Abstract

High crystalline quality titanium disilicides were formed by sputter deposition of alternate Ti⧹Si layers at relatively low vacuum (10 −6 Torr) and subsequent annealing at 870°C for 30 min. The films were composed of large grains with strong texturing to the silicon substrate and the sheet resistivity was of the order of

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.