This research work dealt with production of amorphous powder with nominal composition of (Cu55Zr45Al10)97Hf3 (at%). Combining the mechanical milling and alloying, powder of crystalline Cu-Zr-Al alloy mixed with Hf elemental powder were milled in order to produce a homogenous and amorphous alloy powder The master alloy and the powders milled for different time were analyzed by X-Ray Analysis (XRD) and Scanning Electron Microscopy (SEM). Particle size distribution and hardness were controlled during milling and at the end of procedure. The milling caused dissolving of the hafnium. The 25 h milling time was the optimal to obtain the Hf containing powder with amorphous structure. However, elemental Hf traces with size below 3 µm were still observed in the powder. After 50 h of milling, such impurity elements as iron, nickel, chromium originating from milling tools (vial, balls) were detected.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.