Abstract

Permeability of helium gas in SiC fiber reinforced SiC composite (SiC/SiC composite) was measured by using a vacuum apparatus consisting two chambers. The SiC/SiC samples were prepared by different methods; polymer infiltration and pyrolysis (PIP), PIP and melt impregnation (MI), hot pressing (HP) and liquid phase sintering (LPS). The measurement of permeability was carried out with pressure of helium ranging from 102 to 105 Pa at room temperature. The permeability of the sample made by LPS method was several orders of magnitude lower than those of the other SiC/SiC composites. The lowest permeability, 4 × 10-11 m2s-1, was observed for the SiC/SiC composite made by LPS using SiC fibers and nano powder of β-SiC. The largest permeability, 5 × 10-5 m2s-1, was observed for the SiC/SiC composite made by PIP. The permeability of the SiC/SiC composite depended on the structures of fiber bundle and matrix, and roughly corresponded to the microscopic structures, i.e. pores and cracks.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.