Abstract
Investigation results of changes in the surface structure and helium accumulation in steel Cr18Ni10Ti at various saturation methods are presented. It is shown that different methods of helium introduction can lead to both different and identical changes in the structure and to forms of helium accumulation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.