Abstract

This paper presents leachate studies on fly ash-stabilised expansive clay liners. Fly ash in different contents (0%, 10%, 20% and 30%) by dry weight of the expansive clay was added to the clay, and the ash-clay blend was compacted as a liner overlying a compacted lateritic clay layer. Deionised water (DIW) and calcium chloride (CaCl2) solutions of varying concentration (5 mM, 10 mM, 20 mM, 50 mM, 100 mM and 500 mM) were used as the permeating fluids in the leachate studies. Chemical analysis of the leachate was performed. For a given CaCl2 concentration, the concentrations of both calcium ion and chloride ion in the leachate decreased up to a fly ash content of 20%, and thereafter they increased when the fly ash content was increased to 30%. Further, for a given fly ash content, concentrations of calcium ion and chloride ion increased with increasing CaCl2 concentration.