High-pressure die-cast Al alloys cannot normally be heated at high temperatures due to the presence of pores containing entrapped gases, which lead to the formation of surface blisters. It has been found that blistering can be avoided by using considerably shorter solution-treatment times and lower temperatures. Experiments with alloys 360 (Al-9.5Si-0.5Mg) and 380 (Al-8.5Si-3.5Cu) have shown that strong responses to age hardening are still possible following these modified solution treatments.[1, 2, 3] For T6 tempers, increases in 0.2 pct proof stress of 80 pct for 360 and 115 pct for 380 have been obtained compared with as-cast values. Using a T4 temper, ductility is improved without any sacrifice in strength.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.