Heat capacity spectroscopy measurements in the frequency range from 1.25 to 12 600 rad/s at the dynamic glass transition in poly(vinyl acetate) are reported. The data are compared to results of dielectric and shear spectroscopy in a comparable frequency range on the same sample. The peaks of the different imaginary parts do not have the same position across the main transition zone. The sequence of the peaks with increasing frequency is as follows: dielectric compliance, entropy compliance, and shear modulus. The distances between the different peaks are 0.3 ± 0.4 and 1.0 ± 0.4 frequency decades, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.