Abstract

There are two sorts of hard spot which appears in the products of die-casting, one is of metallic and the other of non-metallic nature. The former is chiefly of primary crystals of various intermetallic compounds containing iron and manganese, as shown in Table. 1 and Photo. 1, a-h.The latter or hard spot of non-metallic nature has also been detected in some products of diecasting (Photo. 4-Photo. 8), as the causes of which the reaction products between the material of crucible or fire-clays and the molten alloy as well as the slag itself contained in the crude silicon have been pointed out.Some remedies according as the causes of hard spot have been suggested.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.