Abstract

The flow stress in tension and compression has been measured as a function of plastic strain in Mg–2Zn castings with grain sizes ranging from 55 to 340 μm. Hall-Petch parameters have been calculated and are compared to those previously reported. In contrast to the behaviour of pure Mg grain refined with Zr and of hot-worked and recrystallised pure Mg and Mg–Zn alloys, the cast material shows little tension/compression asymmetry of the flow stress. The possible effects of texture and of twinning are noted.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.