Hydroxyapatite (HA) has been used as dental implant material and as bone replacement (in bone reconstruction). Ca/P molar ratio varies with the chemical process used, parameter could determine the clinic application. In the present work, HA was synthesized using the wet chemical process (WCP) and the sol‐gel process (SGP). The efficiency of both chemical procedures was greater than 90%. HA by SGP was more crystalline and porous than WCP, also its cluster are further homogenous. The ICP‐OES technique revealed that the HA by SGP was stoichiometric (Ca/P = 1.67). In meantime, the WCP had the molar ratio Ca/P = 1.56.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.