Abstract

Zinc oxide (ZnO) single crystal was grown, for the first time, by the self-flux method using a high-purity zinc solvent saturated with oxygen. ZnO crystals were successfully grown in the solvent by moving a growing crystal slowly, at about 17 mm/day along a temperature gradient (1.5 °C/mm) in a furnace, from 1050 to 500 °C. Hexagonal single crystals 1–3 mm in length and 0.5–1 mm in thickness were obtained. Energy-dispersive X-ray diffraction, secondary ion mass spectrometry, and photoluminescence confirmed that the purity and crystallinity of the ZnO crystals grown in this work were high.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.