The high-quality CdWO4 crystal of 80–90mm in diameter and 180–200mm long has been grown by Low Thermal Gradient Czochralski technique (LTG Cz). Large area atomically flat CdWO4(010) substrates have been prepared by cleavage. The CdWO4(010) surface is stable in the air up to 600°C. At higher temperatures, the precipitation of WO3 and W19O55 oxides has been detected by RHEED.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.