Abstract

Amorphous ZnSnOx (ZTO) films were prepared using plasma-enhanced atomic layer deposition (PEALD) in a temperature range of 100–200°C. Metal-organic precursors of Sn(dmamp)2 (dmamp=bis(1-dimethylamino-2-methyl-2-propoxide) and diethylzinc were employed as sources of Sn and Zn, respectively, in combination with O2 plasma as a reactant. Sn levels in the ZTO films were controlled by varying the SnO2/ZnO cycle ratio from 0 to 8. According to the growth behaviour of the ZTO film by alternating SnO2 and ZnO PEALD cycles, it was observed that ZnO growth on Sn-rich ZTO film is retarded, whereas SnO2 growth is enhanced on Zn-rich ZTO film. The chemical states of the ZTO films were confirmed by X-ray photoelectron spectroscopy (XPS); the chemical compositions of the ZTO films were characterised by XPS depth profiling. Grazing-angle X-ray diffraction revealed that the PEALD ZTO films possess an amorphous structure, irrespective of Sn levels from 20 to 59at.%. ZTO films with intermediate Sn at.% exhibited smooth surface morphology compared to binary ZnO and SnO2 films. Additionally, the step coverage of a ZTO film deposited on hole pattern with an aspect ratio of 8 and opening diameter of 110nm was about 93%, suggesting the realisation of self-limited growth.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.