By testing the number increase and size growth of surface and bulk laser induced damage in KDP and DKDP crystals, we observe different growth characteristics of surface and bulk damage under multiple 355 nm laser irradiations. The size of the surface damage grows exponentially, but that of the bulk damage does not grow. In contrast, the bulk damage number increases, but that of surface damage does not increase significantly. We attribute the differences to the different formation of the damage initiators and the different damage testing volumes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.