Abstract

Ho3+:Tm3+:BaY2F8(Ho:Tm:BYF) laser crystal was grown by Czochralski method. The technical parameters as follows: the seeding temperature is 955°C; the pulling rate is 0.5mm/h; the rotation rate is 5rad/min; the cooling rate is 15°C/h; the period of growth is 6d. According to the spectra of crystal sample, the strongest absorption peak exists at 781nm, and the absorption cross section is 6.16×10-21cm2. While the strongest emission peak exists at 2056nm with the FWHM of 38nm, and the emission cross section is 4.05×10-21cm2, and the emission mechanism at 2056nm was analyzed based on energy level diagram of Ho3+ and Tm3+ ions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.