Abstract
Neodymium doped terbium aluminum garnet (Nd:TAG) crystal with dimensions of O30 × 90 mm was grown by the Czochralski method. The Nd:TAG crystal was characterized by X-ray diffraction, IR spectroscopy, absorption and fluorescence spectra, and laser performance test. The strongest absorption peak is located at 808 nm. There are 3 main fluorescence emission peaks located at 1062, 1108, and 1332 nm, respectively. The prepared 3 at % Nd:TAG crystal was pumped by InGaAs laser diode, the pumping threshold was 360 mW, the highest laser output was 310 mW, the light-light conversion efficiency was 32.3% and the slope efficiency was 51.7%.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.