Abstract

YCa4O(BO3)3 (YCOB) is a good candidate nonlinear optical crystal for optical parametric chirped-pulse application. In order to generate the suitable absorption of idler light near 1588 nm, Sm3+ ions with various concentrations are doped into YCOB crystals. SmxY1−xCa4O(BO3)3 (x = 0.05, 0.3, 0.5, 0.75, 1) crystals of high quality have been grown by the Czochralski method. The X-ray powder diffraction, high resolution X-ray diffraction, ICP-AES, density, absorption spectra, specific heat and thermal diffusion coefficient of as-grown crystals were measured. The results show that the as-grown crystals are isostructural with YCOB; the full width at half maximum (FWHM) of the rocking curve of the wafers with different Sm3+ concentrations are all lower than 30′′; the effective segregation coefficient of Sm3+ ion in this crystal is 0.773 with a Sm concentration of 5 at%; the crystals have absorption peaks in the 1400–1600 nm range.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.