Lead germanate thin films have been grown on BK7 and silica substrates, using pulsed excimer laser deposition (PLD) at wavelengths of 193 and 248 nm, from a bulk lead germanate target under various partial pressures of oxygen. The films produced vary in colour from brown, through clear, to yellow, and a parametric study has been undertaken of the film properties as a function of the growth conditions. The measured losses of the lead germanate films grown on glass substrates varied from ∼2.5 to 7 dB cm −1 depending on the oxygen partial pressure used.