Samples were synthesised by solid-state reaction at high temperatures and characterised by X-ray diffraction analysis, colouristic analysis and particle size analysis. Possible MoO3 evaporation at high temperatures was studied by method of thermal analysis. The most interesting sample is SrO–0.65SnO2–0.05MoO3–0.075Tb4O7 which was prepared by calcination at 1500 °C. This powder is single phase, with cubic structure. Colour of the sample is dark green (L* = 46.37, b* = −9.630 and b* = 10.60).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.