Abstract

All-cellulose composite (ACC) was made from sulphite dissolving pulp fibres by using a partial dissolution method with sodium hydroxide/urea (NaOH/urea) solvent at a low temperature. The resultant composites were compared with untreated sheets. The effect of dissolution time (2, 30, 60, 120 and 240 s) were monitored by XRD, FESEM and mechanical tests. The initial fibre structure was transformed into a thoroughly consolidated composite material after a 30 s dissolution time, and the tensile strength was 14 times higher than that of the untreated fibre sheet without affecting strain. At the same time the amount of non-crystalline matrix in the ACC increased, and the apparent crystallinity decreased. Dissolution times of longer than 30 s had no or a minor effect on crystallinity and mechanical properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.