Abstract

Bi2Te3-based materials play a crucial role in solid cooling and power generation, but the rapidly deteriorated ZT with rising temperatures above 450 K severely limits further applications. Here, this paper reports a novel preparation method of annealing treatment for molten ingot, which can enhance the thermoelectric performance of n-type Bi2Te2.4Se0.6 in a wide temperature range. Instead of conventional halides, copper is adopted to regulate the carrier concentration and grain size to optimal levels. During the process of annealing at 573 K for 4h, the number of twins significantly increases and the grains of Cu-doped samples become larger and more oriented. These optimizations lead to higher carrier mobility with similar carrier concentration compared with the sample without heat treatment. The synergistic effects of Cu doping and annealing treatment realize a high average ZT of 0.89 within 300-600 K in n-type Cu0.02Bi2Te2.4Se0.6. Combined with p-type (Bi,Sb)2Te3, the fabricated thermoelectric device exhibits a high conversion efficiency of 6.9% at a temperature difference of 300 K. This study suggests that annealing treatment is a simple and effective scheme to promote the applications of n-type Bi2(Te,Se)3 in a wide temperature range.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.