Abstract
TEM and atom-probe techniques are used in a combined way for the study of straight and serrated grain boundaries in nickel base superalloys such as Astroloy. These two types of boundaries lead to very different mechanical properties. Experimental conditions are discussed. It is shown that the investigation of boundaries which are perpendicular to the tip axis may lead to biased composition data. Concerning serrated boundaries, microanalyses show that boron and a small amount of carbon segregate at grain boundaries, however, zirconium does not.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.