AbstractThe treatment of nanoscopic silica grafted in the blend during the processing of silica‐filled styrene butadiene rubber was performed with silane, introduced at different concentrations, or at a constant concentration with a given length of alkyl chain. From swelling measurements in water and in solvent, the maximum silane content that can be grafted has been calculated as a function of the length of the silane alkyl chains as well as their efficiency to cover the silica surface. The found values are close to the values found in the literature for grafting in solution. Moreover, a direct correspondence between the length of the silane alkyl chains and their concentration has been deduced. © 2005 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 44: 143–152, 2006