Abstract

Grafting reactions were performed in a Haake torque rheometer, according to a central composite experimental design, where the maleic anhydride and peroxide concentrations, rotor speed, and reaction time were varied. The 27 formulations were analyzed by Fourier transformed infrared spectroscopy and melt-flow index measurements (MFI). An increase in peroxide concentration caused an increase in the percentage of reacted maleic anhydride and in MFI. The effect of initial maleic anhydride concentration presented different types of behavior, depending on the peroxide level. © 1999 John Wiley & Sons, Inc. J Appl Polym Sci 74: 247–255, 1999

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.