AbstractNylon 6, 20 denier, monofilaments were grafted with methylmethacrylate and methylacrylate using ceric ion/sulphuric acid as initiator. Grafted nylon samples with different % graft‐on were prepared by varying the reaction conditions. The thermal stabilities of these grafted samples were compared with parent nylon using dynamic thermogravimetry in air at a heating rate of 6 °C/min up to a temperature of 550 °C. The initial decomposition temperature (IDT) integral procedureal decomposition temperature (IPDT) and activation energy (E) values indicated that thermal stability decreased as a result of grafting.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.