Abstract

Biodegradable superabsorbent polymers were synthesized by graft copolymerization of acrylamide (AM)/itaconic acid (IA) onto cassava starch via a redox initiator system of ammonium persulfate (APS) and N, N, N′, N′-tetramethylethylenediamine (TEMED), in the presence of N,N′-methylenebisacrylamide ( N-MBA) crosslinking agent, sodium bicarbonate foaming agent, a triblock copolymer of polyoxyethylene/polyoxypropylene/polyoxyethylene as a foam stabilizer. The acrylamide-to-itaconic acid ratio, the starch-to-monomer ratio, and concentrations of the crosslinking agent and initiator, on the water absorption of the superabsorbent polymers were investigated. The swelling of starch- g-PAM was 39 g g −1 while the starch- g-P(AM- co-IA) with the IA content of 0.02–0.15% mole gave the water swelling value in the range of 70–390 g g −1. By-products of the reaction were removed by water extraction. The starch grafted composites were characterized by FTIR and SEM. Thermal gravimetric analysis was also used for determining the percentage of grafting ratio. Biodegradation of the starch grafted copolymer was carried out using α-amylase. After the α-amylase hydrolysis, the amount of reducing sugar was quantified by DNS method. The hydrolyzed solution gave a negative test with iodine solution and a positive test by Benedict’s solution, an indication of the existence of glucose units.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.