Abstract

In this paper, (1 − x)(K0.5Na0.5)NbO3–xBi(Mg0.75W0.25)O3 (x = 0–0.015) lead-free dielectric ceramics were investigated. XRD analysis certified that the Bi(Mg0.75W0.25)O3 has diffused into (K0.5Na0.5)NbO3 to fabricate a new solid solution. The addition of Bi(Mg0.75W0.25)O3 depressed the orthorhombic–tetragonal phase transition temperature from 210 to 176 °C and tetragonal–pseudocubic phase transition temperature (Curie point) from 419 to 400 °C. As x = 0.005, the ceramics exhibited high relative permittivity (e ~ 1325), low dielectric loss (tan δ < 2.9%) tan δ stability (Δe/e168°C ≤ ±15%) in the temperature range of 168 ~ 369 °C. Especially, the ceramics also showed optimized piezoelectric constant (d 33 = 122 pC N−1) and remnant polarization (Pr = 32.57 μC cm–2). These results indicated that the BMW added ceramics have potential applications in ferroelectric and thermal stability devices.