Abstract

Data sources Electronic search through PubMed (Medline), CENTRAL (Cochrane) and Embase databases in November 2021. Grey literature searches (OpenGrey, Pro-Quest, National research register and the register of clinical studies hosted by the US National Institute of Health).Study selection Randomised in vivo clinical trials (RCTs) with at least two-year follow-ups, that compared the longevity of adhesively luted indirect ceramic restorations against conventionally cemented indirect metal restorations. The teeth studies had to be about single tooth restorations, on premolars or molars, with sufficient information available for extraction; eg outcome assessment, reason for failure. No language or time restrictions were applied.Data extraction and synthesis Two authors performed study selection, data extraction and quality assessment independently and in duplicate. The following clinical data was extracted: number of participants and dental health status, location of the cavosurface margin, cavity type, reason for intervention, methods and materials for treatment, follow-up, lesion activity at moment of restoration placed, lesion extension (surfaces of restoration), lesion margin (enamel or dentine). It was decided if the restoration was renewed, repaired or re-cemented, then this was classed as outcome failure. Grading of evidence was performed according to the GRADE network.Results After duplicates were removed, 2,667 underwent title screening, 389 abstract screening, and 186 went on to have full text screening with 72 being excluded. In total, 110 eligible articles were then excluded from the 114 that were assessed leaving four RCTs meeting the eligibility criteria and being included in the synthesis, published between 2000 and 2013. Two studies were parallel-arm, the other two, split-mouth design. Overall, 443 restorations had been placed, 212 were adhesively luted ceramic, and 213 conventionally cemented metal restorations; these were all gold. The follow-up periods ranged from 5-7 years. Two studies compared inlays only, one looked at partial crowns only, and the fourth full crowns. The lowest failure rates were found for metal restorations, ranging from 0-11%. The failure rates for ceramic inlays and partial crowns were 5-9% over the same observation period. The failure rates for ceramic full crowns were 36% after five years. The most common failure for ceramic was found to be fracture of the restoration, whereas caries was the most frequent cause of failure for the gold restorations.Conclusions The risk of bias was high for all four studies and the grading of evidence showed a low level of evidence. Only one meta-analysis could be performed comparing conventionally cemented metal vs adhesively luted ceramic restorations, showing the relative risk to fail for conventionally cemented metal indirect restorations is significantly lower than adhesively luted ceramic indirect restorations.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.