Gold flotation concentrate may contain relatively high concentrations of valuable metals such as iron, copper, and zinc, and occasionally, even precious metals such as gold. The major components of the concentrate are SiO2, Fe2O3, and Al2O3, but it also contains reactive sulphide minerals such as pyrite. The sulphides in the flotation concentrate are fully converted into an oxide form during oxidative roasting, therefore, the chemical composition of the roasted concentrate is considered to be a copper slag. High temperature smelting with additives to dissolve Au from the gold concentrate into a molten copper was used in the research. Gold greatly dissolved at 1600?? under a CaO/SiO2 ratio of 1.25, suggesting the increase in the dissolution of gold into molten copper with decreasing viscosity of the molten slag-like concentrate at high temperatures.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.