Abstract
Abstract The glass forming ability (GFA), thermal stability, non-isothermal crystallization kinetics, and mechanical property of Zr 61.5 Al 10.7 Cu 13.65 Ni 14.15 glass forming alloy were investigated. Its maximum glass forming dimension reaches up to 5.5 mm and its critical cooling rate is less than 40 K s −1 . The apparent activation energies for glass transition E g , onset crystallization E x , and crystallization peak E p are 214.56 ± 16.14, 267.42 ± 9.36, and 305.69 ± 7.31 kJ mol −1 , respectively. Small fragility parameter m about 17 indicates its better thermodynamic stability and GFA. In addition, its elastic strain limit, compressive strength, and Young's modulus are 2.73%, 1.81 GPa, and 70.47 GPa, respectively. Its V-shape fracture mode is different form other bulk metallic glasses.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.