Abstract

Amorphous ribbons of approximate composition 0.13Na2O-0.30BaO-0.30Fe2O3-0.27SiO2 were successfully fabricated using roller-quenching, after melting at 1400‡C. Devitrification of the amorphous phase by annealing at 710‡C for 2 h formed a uniform distribution of barium ferrite (BaFe12O19) particles with a mean diameter of 55.88 nm. Other crystalline phases formed on heat treatment were BaFe2O4 and Na2Ba2Si2O7. Devitrified ribbons showed a saturation magnetization (MS) of 24.41 emu g−1 and a coercivity (HC) of 3.06 kOe.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.