Abstract

For many practitioners, longevity of full glass ceramic crowns in the posterior area, molars and premolars, remains a real challenge. The purpose of this article is to identify and evaluate the parameters that can significantly influence their resistance when preparing a tooth. The analysis proposed in this article relies on interrelated studies conducted at three levels: in vitro (mechanical tests), in silico (finite elements simulations) and in vivo (clinical survival rates). The in vitro and the in silico studies proved that an appropriate variation of the geometric design of the preparations enables to increase up to 80% the mechanical strength of ceramic reconstructions. The in vivo clinical study of CAD/CAM full ceramic crowns was performed in accordance with the principles stated within the in vitro and the in silico studies and provided a 98.97% success rate over a 6 years period. The variations of geometric design parameters for dental preparation allows for reconstructions with a mechanical breaking up to 80% higher than that of a non-appropriate combination. These results are confirmed in clinical practice.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.