Abstract

In this work, CaCu3Ti4.7O12 (CCT4.7O) powder was prepared by polymer pyrolysis method. The influence of phase composition and microstructure were characterized using X ray diffraction (XRD) and scanning electron microscopy (SEM). The results show that the TiO2 secondary phase has a remarkable on the microstructure, dielectric loss tangent (tan and dielectric constant () of CCT4.7O ceramics, respectively. Interestingly, low loss tangent of ~0.03 and giant dielectric constant of 31,908 with temperature coefficients less than ±15% in the temperature range of −50–90 oC are observed in a ceramic sintered at 1060 oC for 10h (CCT4.7O-2). Both of ceramics sintered at 1060 oC for 6h (CCT4.7O-1) and 10 h (CCT4.7O-2) display a non linear current voltage with the non-linear coefficient () and breakdown field (Eb) values of 6.4, 5.6 and 1554, 1020, respectively. The dielectric constant, electrical response of grain boundaries, and related nonlinear currentvoltage behavior are found to be associated with the microstructure of CCT4.7O ceramics.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call