Abstract

The geometry effect on the bulk magnetic properties of MnZn ferrite toroidal cores produced by the ceramic method was investigated. The MnZn ferrite powder was pressed at two different toroidal sizes and sintered, under controlled atmosphere at different temperatures. The MnZn ferrites cores were characterized according to their magnetic losses, electrical resistivity, initial permeability and Curie temperature. The total loss (200 mT, 100 kHz) in the small cores S (aspect ratio (AR)=2.84) is lower compared with the total loss in the large cores L (AR=0.79). These results show an agreement with the geometry effect observed on electrical steels.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.