Abstract

We analyzed the failure characteristics of the metallic glass Co43Fe20Ta5.5B31.5 (at.%) deformed in bending. The nanoscale fracture surface morphology respects the micromechanisms of the failure of the amorphous structure. The fracture surfaces consist of nanosized dimples (40 nm) arranged in the lines respecting the periodic corrugation zones oriented perpendicular to the crack propagation direction. The corrugation topology exhibits the point nature of the generation site, the concentric form of the stress waves and their interference.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.