A pulse laser on a phosphate glass activated by Cr3+-Yb3+-Er3+ ions (λ = 1.54 μm) was used to pump Y2Al5O12:Er3+ (YAG:Er) crystals to the lower laser level of a 3-μm transition (4I11/2 → 4I13/2) in Er3+ ions (λ = 2.94 μm). For a pumping pulse energy of Eexc = 200 mJ, the efficiency of 3-μm lasing was 20%. A differential efficiency of the YAG:Er laser in the case of a resonance pumping into the lower laser level amounted to 26%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.