This paper discusses the x-ray luminescence properties of Gd2O2S:Pr:Ce ceramic as a function of its chemical composition. It is established that heat treatment of the ceramic in air affects its x-ray luminescence parameters. A Gd2O2S:Pr:Ce ceramic has been fabricated that possesses weak phosphorescence—less than 20×10−6 of the initial luminescence intensity in 500 ms.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.