Abstract

Optimization of polyaniline (PANI) coating on mild steel (MS) surface has been studied in 0.3 M aniline + 0.2 M sodium potassium tartrate (Na-K Tartrate) by galvanostatic polarization. The current densities of 0.5, 0.75. 1 and 2 mA cm-2 are used for the electrodeposition of PANI on MS. The obtained PANI coatings have been characterized for its morphology using an optical microscope and corrosion performance by using potentiodynamic polarization in 0.4 M Na2SO3 solution simulating an industrial environment. The results reveal a sequential process of dissolution of MS, passivation of MS by forming tartrate salt followed by oxidation of aniline monomer and subsequential nucleation and growth of PANI coating. It is found that the PANI coating obtained at 0.5 mA cm-2 results in better coating producing corrosion inhibition efficiency (IE) of approximately 90% compared to IE of about 75% for coating obtained at 2 mA cm-2.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.