Abstract

Microchip lasers have produced single-frequency, gain-switched pulses with a FWHM as short as 760 psec for Nd:YAG (Nd(x)Y(3-x)Al(5)O(12)) and 80 psec for LiNdP(4)O(12) (LNP).