Abstract

Zircon samples from Ubon Ratchathani, Thailand; Rattanakiri, Cambodia and Dak Nong, Vietnam change their color from light brown and reddish-brown to blue color after thermal enhancement at 1000 ๐C in reducing condition for 60 min. The high temperature is one of the factors for the zircon structure to recrystallize. The objective of this study is to describe the crystal structure of zircon samples before and after thermal enhancement. Zircon is a metamict mineral whose structure is destroyed by some trace elements. There are radioactive elements such as U and Th in the zircon structure. In this study, Raman spectroscopy was used to analyze the molecular vibration in zircon structure before and after thermal enhancement. As a result, the Raman spectra of zircon samples after thermal enhancement show the Raman shift at peak position of V3(SiO4) stretching around 1008cm-1to higher wavenumber concerning to the full width at half maximum (FWHM) values calculated by PyMCA software. The results could be summarized that the metamict zircon will be recrystallized to the crystalline zircon after thermal enhancement. The advantage of this study is about the identification of zircon before and after thermal enhancement.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.