Abstract
In order to fundamentally understand the effect and mechanistic aspects of non-stable cathodic polarization (NSCP) on stress corrosion cracking (SCC) of pipeline steels, square wave polarization (SWP) was employed to investigate the interference of NSCP on SCC behavior of an X80 pipeline steel in a near-neutral pH environment. It was found that alterative stages of SWP, i.e., pulse current and stable current period, play different roles in SCC. The former mainly contributes to the local anodic dissolution (AD) process, while the latter strengthens the process of cathodic hydrogen evolution, thus resulting in increased susceptibility to SCC. Essential electrochemical processes involved above were analyzed in combination of physical and electrochemical models.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.