Abstract

High strength mortar using coal gasification slag fine aggregate were examined. As a result, the higher the replacement rate of the coal gasified slag fine aggregate, the slightly higher the flow value of the mortar. And, due to the increase in the replacement rate of coal gasified slag fine aggregate, the compressive strength of mortar decreased in the high-strength region and increased in the general strength region. Furthermore, even under the condition that the replacement rate of coal gasified slag fine aggregate was 100%, it was possible to obtain a compressive strength exceeding 100 N/mm2.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.